IMG_0060

Dry Pack

ARCHIVE DOCUMENT
Not stated
Unknown
Start of document

DRY PACK

BOWEN/LAYFIELD

Q You refer to the strength of the dry pack. Is there
anything you wish to add to that?

A Yes. I believe I may inadvertently have got wrong
information on the strength of this dry pack, because
Phillips Consultants state that both the filling and the
in situ joints between elements and the dry mortar
packing was 5,700 lbs/sq.in. at 28 days. I presume this
means that all the filling was at the highest strength.
[illegible]

Q Or designed to be at that strength?

A Designed to that strength.

Q And then you say that 'the same dry pack takes the full
load of the entire flank walls and half the floor panels
above it'. Is there anything you want to add to that
comment at this stage?

A No. It takes the load it was intended to take.

******************************

15 page 38 Have you seen any dry pack fillings on the site? (WRIGHT)

A I saw a little on the edges of certain floor panels - such
a little as to be in my opinion a cause for concern. I would
have expected to find quite a lot if the bond betwenn the
factory concrete and the in situ concrete had been first-class.

End of document